Abstract
The Tm3+ laser efficiency of NaGd(MoO4)2 crystals (η=50.8%, Pout=641mW) grown in Na2MoO4/Na2Mo2O7 flux is larger than that obtained in similar Czochralski-grown crystals annealed to eliminate color centers.
© 2011 Optical Society of America
PDF ArticleMore Like This
M. Rico, X. Han, C. Cascales, and C. Zaldo
AWA13 Advanced Solid-State Photonics (ASSP) 2011
Andreas Schmidt, Simon Rivier, Uwe Griebner, Valentin Petrov, Xiumei Han, José M. Cano-Torres, Alberto García-Cortés, and Carlos Zaldo
CThFF2 Conference on Lasers and Electro-Optics (CLEO) 2008
Mauricio Rico, Xavier Mateos, Junhai Liu, Uwe Griebner, Valentin Petrov, José María Cano-Torres, María Dolores Serrano, Carlos Zaldo, Francisco José Valle, Miguel Galán, and Gregorio Viera
WB2 Advanced Solid-State Photonics (ASSP) 2007