We generated 115 mJ of OPO energy at 2 μm from a two-crystal, two-pass, walkoff- compensated KTP pumped multimode at 1.06-μm. The phase matching angle for degeneracy in the X-Z plane of flux grown Chinese KTP is found to be 50.25 ± 0.25°, smaller than previously reported for KTP.