Abstract
2.79 μm Cr,Er:YSGG pumping of a CdSe OPO yielded a 59% slope efficiency (η) and 1.2–2.4 mJ of total idler output between 8.5 and 12.3 μm. A ZnGeP2 OPO operated with a lower threshold, η = 29%, and 0.7–2.4 mJ of forward idler output from 6.9 to 9.9 μm.
© 1997 Optical Society of America