Abstract
A 2.2m long sample of lead-silicate W-index profile fiber with nonlinear coefficient of 820W−1km−1 and exhibiting low and flat dispersion across the C-band is used in an all-optical 160-to-40Gbit/s demultiplexing scheme based on four-wave-mixing.
© 2011 Optical Society of America