Thermal Shock During Cooling/Rinsing of Optical Glass

Not Accessible

Your library or personal account may give you access

Abstract

We measured the thermal shock fracture and strength degradation of the commercially available BK-7 borosilicate crown optical glass as a function of surface finish prior to thermal shock testing and amount of temperature drop in de-ionized water and a more viscous silicone oil. There is little strength degradation for temperature drops smaller than critical. Post-quenching strength depends on surface finish and the cooling/rinsing medium.

© 2010 OSA, SPIE

PDF Article
More Like This
Optical trapping and cooling of glass microspheres

Tongcang Li, Simon Kheifets, David Medellin, and Mark G. Raizen
FTuN2 Frontiers in Optics (FiO) 2010

Thermally Induced Fracture of Laser Glass in High Average Power Gas-Cooled Laser Systems

E. Sistrunk, F. Batysta, J. Benge, F. Cebreros, A. Church, J. Galbraith, T. Galvin, D. Keebaugh, E. Koh, R. Kupfer, E. Lowell, W. Maranville, S. Mitchell, J. Peterson, B. Reagan, L. Sawyer, K. Schaffers, I. Tamer, D. Willard, and T. Spinka
SM1D.4 CLEO: Science and Innovations (CLEO:S&I) 2023

Development of Nd-doped Optical Gain Material Based on Silica Glass with a High Thermal Shock Parameter for High-Average-Power Laser

Yasushi Fujimoto, Takahiro Sato, Hajime Okada, Kazuhiko Sumimura, Hidetsugu Yoshida, Masahiro Nakatsuka, Tetsuji Ueda, and Akira Fujinoki
CTuQ7 Conference on Lasers and Electro-Optics (CLEO:S&I) 2005

Select as filters


Select Topics Cancel
© Copyright 2024 | Optica Publishing Group. All Rights Reserved