Abstract
The strongest absorption in Yb:(Gd1-xYx)2SiO5 crystals obtained by Czochralski method blue-shifted from 978nm in YSO phase to 920nm in GSO phase. Crystals with YSO phase displayed broader emission bandwidth than that with GSO phase.