Abstract
Ultrathin (≥0.5 nm) adhesion and capping layers were used to inhibit dewetting in 50 nm Au thin films. A 1500x stability enhancement was found over standard 2 nm adhesion Ti layers used in HAMR.
© 2018 The Author(s)