Transmission spectra of standard military and commercial paints were measured, and the best transmission zone was found in the middle-IR from 3.5-um to 5.7-um. Middle-IR backscattering scanning and CCD imaging approaches were developed to detect metal corrosion and small cracks underneath paint layers of up to 150-um.