Time-Integration holograms, where the exposure pattern is recorded as a sequentially applied sum of individual fringe patterns (either sinusoidal "Young’s" fringes or Gabor zone plates), suffer from poor diffraction efficiency and, consequently, low signal-to-noise ratio on reconstruction [1,2]. The reason is straightforward: The total exposure pattern, as in the case of incoherent holography [3], has a low signal-to-bias ratio when many contributing exposures--each bringing its own bias with it--are applied. Since the recorded signal exposure is low compared to the bias exposure, the signal variations in the wave amplitude transmittance function of the processed hologram are small, and diffraction efficiency is therefore low. At the same time, noise in the reconstruction, determined by such sources as dust- and film-grain-scattered light, remains at an essentially constant level.

© 1986 Optical Society of America

PDF Article
More Like This
Diffraction efficiency limitations of holograms recorded in silver halide emulsions

A. A. Ward, L. Solymar, and U. Oxford
FV10 OSA Annual Meeting (FIO) 1986

Theoretical model of reconstructed scatter noise in silver halide holograms

G. D. G. Riddy and L. Solymar
FV8 OSA Annual Meeting (FIO) 1986

Multiply Exposed Photorefractive Holograms With Maximal Diffraction Efficiency

David Brady, Ken Hsu, and Demetri Psaltis
PD2 Optical Computing (IP) 1989