Abstract
The Verdet constant of a 0.8 at.% Ti-doped TAG ceramic was investigated between 5 and 296 K. A high value of the Verdet constant was obtained as 184.2 rad/Tm at 296 K for 632.8 nm.
© 2015 Optical Society of America